The following of the test report of the laminated glass made with EVA film.

The laminated glass samples is :4mm thickness glass+0.38 EVA FILM+4MM glass.

But note that different EVA film manufacturers in China has different formula of their EVA film product, so the following is for reference, for exact statics, please contact your EVA film suppliers in China.

[-visible light transmittance 90%

-visible light reflectance 9%

-Sunlight total transmittance 88%

-Sunlight direct transmittance 85%

-sunlight direct refectance 7%

-uv transmittance 3%

-shading coefficient 0.99

-heat transfer coefficient 5.7w(square meter*k)]

All rights reserved by China Ethylene-vinyl acetate EVA Interlayer Film Manufacturer for Safety Architectural Laminated Glass, Smart Glass, Privacy Glass, LED Glass etc.(cnc@cncnext.com / www.cncnext.com / benext77@gmail.com / benext77@hotmail.com) (eva@evafilms.com / www.evafilms.com )

+China Silicone Vacuuming Bag manufacturer for EVA Glass Laminating Machine/Privacy glass laminating

+China Silicone Sheet Manufacturer for Solar EVA Photovoltaic Panel Encapsulation

(uc@ucolin.com / www.ucolin.com /umewe360@gmail.com/umewe360@hotmail.com)

Published by cnc@cncGlass.com www.cncGlass.com EVA film glass interlayer

cnc@cncGlass.com www.cncGlass.com EVA film glass interlayer